What you have so far looks really good.
I would recommend working some more on the spots of pitting you have left. It wont take much more to get that taken care of and of course the end results will be much better if you do. However, i do not know how much material has already been removed and without you knowing how much you have to work with, it should be handled with caution. You would be amazed as to how much pitting can be removed by only removing a few thousanths of metal.

These are damascus, right? If so, a proper black and white finish must be done to obtain the contrast. Not just a simple rust blue (which will be all black).

If you dont want to mess with doing the black/white yourself, i would recommend NO ONE else currently than Dale Edmonds to do it for you.
__________________
B. Dudley
Brian Dudley is offline   Reply With Quote
The Following 2 Users Say Thank You to Brian Dudley For Your Post:
Visit Brian Dudley's homepage!
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 11:27 PM.

Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Parkerguns.org
Copyright © 2004 Design par Megatekno
- 2008 style update 3.7 avec l'autorisation de son auteur par Stradfred.