Unread 06-09-2017, 12:09 PM   #21
Member
Bill Graham
PGCA Member

Member Info
 
Join Date: May 2016
Posts: 291
Thanks: 234
Thanked 223 Times in 64 Posts

Default

Quote:
Originally Posted by Brian Dudley View Post
Multiple brownings before boiling is more like the "Parker process" that Gaddy wrote a separate article on. This process had a boiling in logwood and ferrous sulfate at the end.
In one of the records of Dr. Gaddy's account of the Parker Process, it states 7-10 rustings before converting the rust. Then the process states to etch for 5 minutes, and then you should be able to rub off with a finger tip what the etchant removes. Does this sound right? That's a lot of bluing done before the etching, so maybe 5 minutes is required.

I've got two sets going now. One I'm doing this way, the other is being done the other way Dr. Gaddy articulated, which is rust, boil, etch, rust, boil, etch, etc. I tried it multiple ways, with different variations here and there, but for these I'm going to be very strict and do a comparison between the two processes.
Bill Graham is offline   Reply With Quote
The Following 3 Users Say Thank You to Bill Graham For Your Post:
Visit Bill Graham's homepage!
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 04:55 AM.

Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2025, Parkerguns.org
Copyright © 2004 Design par Megatekno
- 2008 style update 3.7 avec l'autorisation de son auteur par Stradfred.