After my last post, I decided Bruce is right, in that the parts, after the normalizing cycle at 1650-1700 degrees, get a temper/stress relieving cycle, at under 1125 degrees, in a controlled atmosphere furnace, and not in the boxes they are normalized in.
Dean is correct. They are individually heat treated. The secret to the color is in the packing, and composition of carbon bearing packing material.
I never hear anyone mention it today, but one of the old materials was horse manure. No $hit !