Thanks, Art. I had some 0000 pumice on hand but haven't used it as I was afraid it was coarser than rottenstone. Looking at the just finished stock set, as it final dries, I see some uneven areas of reflection, so I'm thinking a final rubdown with the finish and rottenstone will even it all out.

Again, I appreciate it!