Is a wall thickness of 0.0519685 [1.32mm] at the muzzle acceptable for firing, assuming there is no serious pitting?


Quote:
Originally Posted by Brian Dudley View Post
It is not too uncommon. I recently had a 12g C grade hammer gun in my shop with 10g boring. Built that way.