This is extracted from an article I have here by Tom Armbrust

The load is: Winchester 12 gauge 2 3/4" Hull 17.0 grains IMR 700-X
powder with a Greenduster GT Wad #9210-12

Primer Velocity FPS Chamber Pressure

Fed 209A 1251 10,860

CCI-209M 1248 10,460

Win. 209 1246 10,140

Rem. 209 STS 1236 9,740

FIO-616 1234 9,690

CCI-209 1232 9,650

Rem. 209P 1228 8,810

Fed 209 1226 9,070

Win 209 MDL 1224 10,200

Cheddite 209 1217 9,270


The bad thing is, if you try this same test with a completely different load, in say 16 gauge. Those primers will be in different locations. I've tested enough loads to know that they will act differently in different loads. Sure, you're magnum primers will always be at the top. But the others will move around. If you're not following a specific tested load, the only way you'll know for sure how a primer swap will change the load, is to have it tested.