Quote:
Originally Posted by Brian Dudley
The channel in the plate for the unhooking slide results in a dramatically different thickenss of material up the middle of the plate. This is really the main reason for a difference in the appearance and patterning of the colors in that area.
|
True Brian, and the variation in thickness of the plate where that channel is machined results in the variation in temperature across the width of the plate I made reference to.
As I recall, you send your case coloring work to DTR and they are expert in the various case colors of the various gun makers of old.
Dave Trevallion showed me his 20 gauge Trojan he had restored himself and sent it to Doug to color case harden. I honestly believed it was a very high condition original, stripe on the floor plate and all. David told me that Doug had done it fifteen or more years earlier. I was really surprised but shouldn’t have been, knowing the accuracy of Doug’s work.
.