Well then maybe these will work.

Winchester AA Hull = Lead Shot 12ga 1 1/4 oz. 800-X 27.5gr Rem. 209P primer Rem. SP12 wad 7,800 PSI 1275 fps

Winchester XPert Hull = Lead Shot 16ga 1 1/8 oz. SR 4756 23gr Rem. 209P Rem. SP16 wad 8,900 PSI 1150 fps