Thread
:
Pressure Test for 19gn Red Dot
View Single Post
07-30-2020, 04:25 PM
#
1
Member
Gary Laudermilch
Forum Associate
Member Info
Join Date: Feb 2010
Posts: 1,330
Thanks: 3,049
Thanked 2,113 Times in 676 Posts
Charlie, the components did not change. Just the hull. According to the ballisticians at the time, the difference was in the composition of the plastic used in the hulls. Federal plastic being more elastic.
The Following User Says Thank You to Gary Laudermilch For Your Post:
Mike Koneski