That one may have been done by Color Case Company in Ohio. They did a fairly nice job of cyanide coloring back in the day. Unfortunately they went out of business several years ago.

I'm not sure if you could just get the floor plate done using the traditional bone hardening process. I'd be afraid the plate would warp from the heat if it wasn't attached to the frame in the process.