Thread
:
Salt Proofing Parkers
View Single Post
12-22-2014, 05:45 PM
#
3
Member
C grade
PGCA Lifetime
Member
Member Info
Join Date: Nov 2008
Posts: 1,390
Thanks: 4,135
Thanked 1,248 Times in 457 Posts
Mills
I have a DHE I use. I had the inside packed with grease to keep out the elements. I am told this is an old time solution. I then use BLU corrosion preventative on all exposed metal. It has worked well so far.
David
The Following User Says Thank You to David Dwyer For Your Post:
Mills Morrison