Dean,

The concern with Hevi-shot (tungsten, nickel, iron) is the hardness which is harder than anything else (much harder than steel) and permanently marking and wearing the softer composition damascus or twist.

But if it is contained inside a shot cup??? Large charges have shot outside the shot cup in factory loads.