| Notices |
Welcome to the new PGCA Forum! As well, since it
is new - please read the following:
This is a new forum - so you must REGISTER to this Forum before posting;
If you are not a PGCA Member, we do not allow posts selling, offering or brokering firearms and/or parts; and
You MUST REGISTER your REAL FIRST and LAST NAME as your login name.
To register:
Click here..................
If you are registered to the forum and keep getting logged
out: Please
Click Here...
Welcome & enjoy!
To read the Posts, Messages & Threads in the PGCA Forum, you must be REGISTERED and LOGGED INTO your account! To Register, as a New User please see the Registration Link Above. If you are registered, but not Logged In, please Log in with your account Username and Password found on this page to the top right.
Hi Unregistered,
On July 29th, this site will be moving..! No, really - it's "moving" to another physical location - including servers, gateways, routers - everything - including my coffee cup...
So, from the date of July 29th through July 30 or 31 (shooting for these dates, but - as always, I'm at the mercy of my ISP who has to install the lines to the new location - and we actually get them running ;) ). But - this site, cloud servers and main web will be OFF LINE.
Now, please save these dates!! Please - don't be "that guy" who emails me on the 30th to tell me you "can't open the Parker Website". I'll already know it is offline - and also know that you are "that guy"...
I'll take this notice up and down over the next week or so - and leave it up during the final few days before shutting it off on the 29th..
John D.
|
08-07-2013, 09:32 AM
|
#24
|
Member
|
|
|
Member Info
|
Join Date: Nov 2008
Posts: 4,995
Thanks: 554
Thanked 15,715 Times in 2,677 Posts
|
|
I guess I'm confused. The Formby's I use says on the can that it is a varnish made from tung oil and other penetrating oils. That is what I read and it was recommended so I bought and used it. I did not understand it to be pure tung oil and who knows, pure tung oil may not be the right stuff to use. I figure Formby's knows more than I do about producing an effective finish.
I think it does an acceptable job of making a mat surface look shinier, feel smoother and bringing out some detail.
Yet we have one person contending that it contains absolutely no tung oil and another another talking about "bullpucky" and all couldn't be trusted as fact.
Maybe somebody could explain what all this is about and what it wrong with Formby's etc. If there is a better magic stuff to use, please educate me.
|
|
|
|
| Thread Tools |
|
|
| Display Modes |
Threaded Mode
|
Posting Rules
|
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts
HTML code is Off
|
|
|
All times are GMT -4. The time now is 07:01 AM.
Powered by vBulletin® Version 3.8.4 Copyright ©2000 - 2026, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2026, Parkerguns.org Copyright © 2004 Design par Megatekno - 2008 style update 3.7 avec l'autorisation de son auteur par Stradfred.
|