Unread 10-15-2018, 07:29 PM   #20
Member
OH Osthaus
PGCA Lifetime
Member
 
Rick Losey's Avatar

Member Info
 
Join Date: Jul 2010
Posts: 7,808
Thanks: 1,646
Thanked 8,157 Times in 3,260 Posts

Default

Quote:
Originally Posted by Paul Harm View Post
I have a question. I've read on another web site that there is color case hardening and case coloring. The second one is done at a temp, but not enough to case harden the parts. It's more of a chemical process. It was also said that Turnbell [ along with at least Pietta ] uses the second process, but no talk if they also used a hardening process. Can anyone shed any light on this ?
TURNBULL replicates case colors which is an attractive result of the hardening process . The process involves bone charcoal and heat and skill


an after thought- some later case color was done with a cyanide process- its a boiling process so not as much heat and little if any hardening
__________________
"If there is a heaven it must have thinning aspen gold, and flighting woodcock, and a bird dog" GBE
Rick Losey is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:55 AM.

Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Copyright © 1998 - 2024, Parkerguns.org
Copyright © 2004 Design par Megatekno
- 2008 style update 3.7 avec l'autorisation de son auteur par Stradfred.