And one more while I'm at it: I may go ahead and order some Cheddite hulls. They come primed with ch209 primers. I don't know how different they are from the Winchester 209, but does anyone have a 7/8 or 1 Oz recipe for that combo? I currently have the Claybusters WAA 16 wad, and the SP 16 wad, but will also be getting some DR 16's. I am making a trip to "the big city" in the next few days and plan to stock up on all the things I can't get here.

This info would help until I hear back from the low pressure group and get their data tables.