Originally Posted by Dave Miles View Post
I have a couple loads, that I had tested by Tom Armbrust.


New 2-1/2" Cheddite hull. Can be purchased from Graff's and sons.
It comes primed with Cheddite primer, but you can use Win. 209 after.
20 grains International Clays
GU-1222 wad. can also get from Graff's.
1 oz. lead shot
1200 FPS @ 6800 PSI
If you adjust your reloader correctly, you'll get perfect crimps,
with either 6 or 8 point crimp.

You can also use:
21 grains of IMR-PB for 1125 FPS @ 6000 PSI
22 grains of IMR-PB for 1225 FPS @ 7200 PSI
These loads were also tested.
Regards, Dave

Opps, I guess they're out of stock right now.
http://www.grafs.com/product/256611
But, you can cut down the 2-3/4" Cheddite hulls.
Dave,

Any reason to think these numbers would be radically different substituting bismuth for the lead??

BP