A 1983 DuPont reloading guide shows a number of options, depending on case/primer and wad, but they generally use 23 or 23.5gr of 800X. AA case with 209 primer WAA12F1 wad and 23 grains of 800X results in 1195 fps and pressure (LUP) of 5900. Many more loads with 1 1/8 oz shot.

I'm going to try a couple of boxes of this recipe on clays later this week. I'll report on my findings.

If you have a specific combination you are interested in, PM me, and I'll see if it's in the guide.