Here is how I would address that stock……..I would very lightly sand the whole stock so that the color is the same. I would then fill the open pores with the mud method using multiple iterations of tung oil as a pore filler. It should take about three iterations. Then you can finish up with Timberlux wiping down each iteration with a clean cotton cloth building microscopic layers till you get the look you want. I would probably do the same to the forend so that all matches.