Originally Posted by Bruce Day View Post
What I have learned is that the crucibles containing the various parts are not subjected to the same furnance time.
Are you certain of that? I received regular orders from Colt, in West Hartford for these "crucible". In the case of Colt, they were a 5x5x10" box, cast in a martensitic alloy (called CA6-NM, for those that care) I have been in the heat treating department at Colts many times, and, at least in their case, the boxes aren't unclamped until back to room temperature.
edgarspencer is offline   Reply With Quote